Description Tensile Strength  Impact Strength Heat Deflection
ABS 6,100 psi 2.7-7.7 ft-lbs/in 203-214° F
ABS-Flame Retardant >5,500 psi 4 ft-lbs/in 194° F
Acetal 20% Glass Filled / Delrin 570 8,500 psi 0.8 ft-lbs/in 316-345° F
Acetal Copolymer 8,800 psi 1.0 ft-lbs/in 230-316° F
Acetal Homopolymer / Delrin 150 9,000 psi 1.5 ft-lbs/in 257-336° F
Acetal Static Dissipative / Tecaform SD 6,600 psi 1.8 ft-lbs/in 190° F
CPVC 7,300 psi 9 ft-lbs/in 198° F
HDPE 4,600 psi 1.3 ft-lbs/in 176° F
LDPE 1,700 psi No Break 160° F
Nylon 6 10,000 psi 0.6 ft-lbs/in 200-370° F
Nylon 6/6 10,000 psi 1.1 ft-lbs/in 194-455° F
Nylon 6/6 30% Glass Filled 12,000 psi 1.0 ft-lbs/in 482-490° F
PC 8,000-9,500 psi 2.0-16.0 ft-lbs/in 270-280° F
PC 20% Glass Filled 16,000 psi 2.06 ft-lbs/in 298° F
PEEK 14,000 psi 1.55 ft-lbs/in 285-482° F
PEI / Ultem 1000 15,200 psi 1.0 ft-lbs/in 392-410° F
PEI 30% Glass Filled / Ultem 2300 24,500 psi 1.6 ft-lbs/in 414° F
PET 11,500 psi 0.6 ft-lbs/in 175-240° F
PMMA / Acrylic 10,809 psi 6.8 ft-lb/in² 185-212° F
PP Copolymer 4,200 psi 1.2 ft-lbs/in 96-195° F
PP Homopolymer 4,800 psi 1.2 ft-lbs/in 210° F
PPE+PS / Noryl 265 9,200 psi 3.5 ft-lbs/in 254-279° F
PPSU / Radel R 5500 10,100 PSI 13 ft-lbs/in 428° F
PS (HIPS) / Polystyrene >3,000 PSI 2.8 ft-lbs/in 185° F
PSU / Polysulfone 10,200 PSI 1.3 ft-lbs/in 345-358° F
PTFE / Teflon 2,900-5,076 PSI 2.0-6.0 ft-lbs/in 500° F
PVC 7,820 PSI 0.8 ft-lbs/in 162-172° F
UHMW 5,800 PSI No Break 116° F